SOLSTICE PTM6000HV
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 0.14 Thermal Impedance
- 5.2 Thermal Conductivity
- Optimized for IGBT
Product Description
PTM6000HV, commonly known as PTM6000HV, is a highly thermally conductive Phase Change Material (PCM) in paste format. This High viscosity(HV) version of PTM6000-SP is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications. It has a very wide process window that makes it an optimal, tailor made option for IGBT printing and honeycomb structures.
PTM6000HV is based on a robust polymer PCM structure and exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. This material exhibits excellent wetting at interfaces during typical operating temperature range, resulting in very low surface contact resistance.
PTM6000HV is a proprietary material that uses a proprietary filler to provide superior reliability (pass 150˚C baking 2000 hours, temperature cycling 2000 cycles, and HAST 288 hours) and maintains low thermal impedance (<0.12˚Ccm2/W no shim), making PTM6000HV desirable for high-performance integrated circuit devices. PTM6000HV has been renamed from PTM6000HV-SP for the sake of simplicity. It is the exact same product.
Reference the PTM6000 Automotive Reliability Report which demonstrates its performance and thermal stability after various long-term reliability tests including HAST 192hrs, T/C-B 4000x and High Temperature Baking of 3000hrs.
Packaging
TDS, SDS & Technical Documents
- Honeywell PTM6000HV SDS - German
- Honeywell PTM6000HV SDS - English
- Honeywell PTM6000HV SDS - Italian
- Honeywell PTM6000HV-SP_SDS - French
- PTM6000HV-SP_SDS_HU
- PTM6000ReliabilityReportRevD
- IGBTprintingprocessguidelines
- HEMTIMApplicationNoteSPtype
- Drying Time of PTM6000HV-SP at Different Temperature
- Drying Time of PTM6000HV-SP Low Viscosity (103 Pa-s) version (2)
- PTM6000HV-SP REACH SDS_EN
- PTM6000HV-SP_REACH SDS_ES
- PTM6000HV-SP_TDS_2025
- CAPLINQ Honeywell Phase Change Material Troubleshooting Guide v2
- PTM6000HV-SP MSDS Dutch
- PTM6000HV-SP under Temp Cycling (-40 to 150C)
- PTM6000HV-SP (Thai)
- PTM6000HV-SP 2 (Thai)
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Additional Information
When choosing a printable paste it is important to understand the process parameters and limitations.
That's why we ask, when you contact us, to include the following information:
- What is your print thickness?
- How long is your printing time and working window?
- What is your drying step after printing?
- Temperature (Room temperature or something else?)
- Time
- Do you have any viscosity limitations in the printing process?
| End of Line |
0.10 °C-cm²/W
|
| Bake 125˚C, 2000 h | 0.09 °C-cm²/W |
| Bake 150˚C, 2000 h | 0.09 °C-cm²/W |
| HAST, 288h | 0.09 °C-cm²/W |
|
Temperature Cycling “B”
(-55˚C to +125˚C, 2000 cycles)
|
0.07˚ °C-cm²/W |

280cc cartridges are intentionally about 90% filled (650g) to allow for room at the top to fit the adaptor/plunger for dispensing.
Other lower filled configurations in 280cc cartridges are possible, if there is sufficient volume or justified with manufacturability concerns.