ALPHA CVP-390V

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

ALPHA CVP-390V Solder Paste

Main features

  • Superior electrochemical reliability
  • Wide process window
  • Reliable post reflows flux residue

Product Description

ALPHA CVP-390V is a lead-free, no-clean solder paste designed to maximize flexibility in manufacturing processes, and provides excellent electrochemical reliability under extreme operating conditions. It exhibits consistent print and reflow performance across a wide range of component types.

ALPHA CVP-390V exhibits >2.00CpK for transfer efficiencies between 60% to 120% area ratios above 0.60 against variable print process conditions. It also maintains repeatable transfer efficiency on fine feature 01005 components and excellent coalescence down to 170um circle and square apertures. 

ALPHA CVP-390V exhibits best-in-class electrochemical reliability down to 0.100mm comb spacing against the most challenging SIR profiles, making it ideal for applications requiring high reliability.

Product Key Features:

  • Superior electrochemical reliability
  • Wide process window
  • Excellent reflow and coalescence

Note: Reading the technical data sheet (TDS) prior to use is highly recommended.

Product Family

231207

500g Jar | Type 4
1. Select Package Type
2. Select Alloy Type
3. Select Particle Size

Loading pricing…

Product availability
EU Shipping in 4 weeks
Packaging
Unit of measure Jar
Net weight 0.5 kg
Gross weight 0.65 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Type
A metallic element type
SAC305 and Innolot alloys

Additional Information

Reflow Guidelines

Capable of reflow in air and N2 environments.


SAC305InnolotStraightRampFigure. SAC305 & Innolot Straight Ramp
HighSoakSAC305Innolot
Figure. SAC305 & Innolot High Soak