LOCTITE ABLESTIK 2033SC

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 2033SC

Main features

  • Low cure temperature
  • Legacy smartcard product
  • Optimized rheology

Product Description

LOCTITE ABLESTIK 2033SC die attach adhesive is designed for high throughput smart card bonding applications. It is compatible with various encapsulant chemistries. This monocomponent low bleed product has long work life and can cure fast at low temperatures, making it ideal for smart-card applications.

Cure Schedule

  • 90 seconds @ 110°C

LOCTITE ABLESTIK 2033SC is a mature and price efficient product. Legacy smartcard products could and should be served by 2033SC. For new applications and snap cure materials though we suggest you take a look at LOCTITE ABLESTIK 2035SC and LOCTITE ABLESTIK 2035SCR.

Product Key Features

  • Engineered to cure quickly at lower temperatures, which minimizes thermal stress on sensitive semiconductor components and accelerates production cycle times.
  • Optimized for automated assembly processes, making it ideal for high-speed, high-volume production lines.
  • Provides superior adhesion and stability under both thermal and mechanical stress, ensuring long-term reliability of the bonded device.
  • Exhibits low bleed characteristics

Applications

  • Smart Card Bonding: Specifically designed for bonding Si dies to PBGA-FR4.
  • Microelectronics assembly
  • High-volume die attach
Product Family

233295

5cc in 10cc Syringe (7g) - 2348519
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 55 days
Packaging
Unit of measure Syringe
Net weight 7 g
Gross weight 15.92 g
Dimensions 3 x 1.9 x 9.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
46 °C
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
6.1
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
11,300 mPa.s

Additional Information

Further Reading on Die Attach Materials

Bare copper

Bare Copper Substrate Die Bonding

Rose Anne Acedera, August 2025
Blog 2 Banner

Optimizing Die Attach Dispensing

George Kountardas, May 2025
Blog 3 Banner

Curing Die Attach in Vacuum

George Kountardas, September 2021

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers